Application

Three spray parameters: distance, pressure, travel speed — get one wrong and the coat is wasted

Spraying looks like the easiest skill to pick up and is where systematic error creeps in most easily. The error does not show immediately; it appears at once in thickness statistics, adhesion and appearance.

1. Distance: 15–25 cm, and constant

Too close: local overthickness, solvent cannot escape, sags and pinholes, and the air blast ripples the wet film. Too far: droplets dry in flight and land as dry spray, particles do not coalesce, and both adhesion and appearance suffer.

The usual mistake is adjusting fan width by moving the gun. Fan width comes from nozzle and cap selection; distance stays constant. Using distance to set pattern changes thickness and dryness at the same time.

2. Pressure: the maker's minimum atomising pressure

Excess pressure is the commonest waste: more overspray (measured losses of 20–30% are typical), faster solvent loss causing dry spray, and a less dense film. Too little pressure gives poor atomisation, orange peel and coarse particles.

Use the maker's minimum atomising pressure and adjust slightly until the fan is even with no coarse particles. With airless, it is about matching pump pressure to tip orifice — not more is better.

3. Travel speed and overlap

There is no absolute speed, but it must match output and fan width so that one pass reaches target thickness. Too fast gives a thin coat, too slow sags. The practical check is wet film thickness immediately after a pass, adjusted from the reading.

Overlap is usually 50%, each pass covering half the previous. Less leaves thin bands, more creates local overthickness. Work top to bottom on vertical surfaces and in one direction on horizontal, without swinging back and forth.

4. The ignored fourth variable: viscosity and temperature

Viscosity varies widely with temperature. No heating in winter and no thinning in summer, run through the same pressure settings, produces completely different results. Control paint temperature, typically 20–25 °C, rather than thinning to compensate.

Thinner is used only within the maker's limit; excess lowers volume solids and leaves the film thin. Half of good spraying is preparation and half is keeping the parameters stable.

Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp