MODEL DATA

Hardtop F10

BrandJotun
ModelHardtop F10
CategoryFluorocarbon topcoat

Hardtop F10 is a Fluorocarbon topcoat from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids40 ± 2%
Dry film thickness25–40 µm
Theoretical spreading rate16–10 m²/L
VOC495 g/L (China)
Density / specific gravity1.2 kg/L
Number of componentsTwo-component
ThinnerJOTUN Thinner No. 10
Mixing ratio17 parts: 1 part (by volume)

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Fluorocarbon topcoats get their weathering resistance from the high bond energy of the fluorine-carbon bond. Under UV they do not age slowly; within the design life they barely age at all. The price is cost, application discipline, and one often-missed fact: adhesion to the substrate is mediocre on its own and depends on the specified primer.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Resin type (FEVE, PVDF and so on) and fluorine contentTypes differ in application route. PVDF usually needs elevated baking, while ambient-cure site work uses FEVE types. Fluorine content drives the weathering term.
  2. Required primer and intermediateFluorocarbon is almost never used alone. With the wrong system, adhesion fails from the bottom up, not at the surface.
  3. Minimum curing temperature and shortest dry timeAmbient-cure types film poorly at low temperature, and both gloss and weathering suffer.
  4. Repair and recoat procedureThe surface energy is low, so repair interfaces need specific abrasion and blending steps that the data sheet describes.

Application control points

Low surface energy means preparation before overcoating

The finish is slick. Repair work without abrasion will not hold. That is the nature of the material, not a defect.

Keep the film thin rather than thick

The value sits in the surface weathering layer, not in thickness. Excess thickness adds cracking and cure risk.

Lock colour and gloss consistency before a phased delivery

On large projects supplied in batches, colour difference shows most on metallics and darks. Reserve one batch or approve a panel first.

How to settle site disputes

Treating fluorocarbon as permanent

Design life is usually stated in decades, but only with a complete system and compliant application. If the primer fails, the best topcoat cannot save the steel.

Repairs that leave visible patches

Gloss retention is so good that old and new areas differ for years. Blend across a full elevation or along a joint line.

Common questions on this coating class

Fluorocarbon or polysiloxane?
Both sit at the top of the weathering range. Fluorocarbon holds gloss and colour more consistently and offers more colours; polysiloxane allows high-solids thick build with fewer coats. Decide on the required term and the site conditions.
Can fluorocarbon be the topcoat in immersion?
Not recommended. Immersion performance depends on barrier and adhesion, where epoxy and glass-flake systems are the better fit.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Typically used as a topcoat for colour, gloss and weatherability; primer and intermediate are selected separately to suit the exposure.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← JOTUN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp