XH6007A is a Polyurethane topcoat from T&H. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 58% |
|---|---|
| Dry film thickness | 60/80/100 µm |
| Theoretical spreading rate | 5.8 m²/L |
| VOC | 410g/L |
| Density / specific gravity | 1.12 kg/L |
| Number of components | Two-component |
| Thinner | 0-20% |
| Mixing ratio | Base: curing agent = 5:1 (by weight), 82:18 (by volume) |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
Polyurethane topcoats rely on the urethane linkage formed when an isocyanate hardener reacts with a hydroxyl resin, which puts weathering and gloss retention at the top of the normal topcoat range. Two sensitivities come built in: the hardener dislikes moisture, and the recoat window is narrow. Both make it far less forgiving on site than epoxy.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Aliphatic or aromaticAliphatic does not yellow and suits exterior and light colours; aromatic is cheaper, weathers poorly and yellows outdoors within months. The data sheet must say which, not merely polyurethane.
- Hardener ratio and pot lifeThe ratio is stoichiometry, not a suggestion. Over- or under-dosing gives poor cure or brittleness. Pot life sets how much you mix at a time.
- Recoat window, minimum and maximumNarrower than epoxy. Past the maximum, intercoat adhesion has to be restored by abrasion.
- Minimum application and curing temperatureReaction rate collapses at low temperature, so products set a floor below which you do not apply. The figure differs by product; read the sheet.
Application control points
Keep hardener containers sealed and mix full units
Isocyanate reacts with atmospheric moisture; an opened can skins over and loses activity. Decanting into small cans creates more problems than it solves.
Do not leave the interval overnight if you can avoid it
Windows exist to give chemical plus mechanical bonding. Coating the next morning means relying on abrasion, which is inferior to recoating inside the window.
Light and dark colours need different thickness discipline
Light colours hide poorly, so crews build thickness to cover and overshoot the spec. Tint the primer or add a coat instead.
How to settle site disputes
Gloss loss and chalking mistaken for a defect
Under strong UV and acid rain, gloss loss is normal ageing. To judge premature failure, compare against exposure time and neighbouring areas, not against the presence of chalking.
False cure from moisture-contaminated hardener
Dry on the surface, soft underneath, fingerprints on pressing. Check ratio and storage before blaming the paint.
Common questions on this coating class
Can polyurethane go straight onto zinc-rich primer?
Is aromatic polyurethane acceptable indoors?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Typically used as a topcoat for colour, gloss and weatherability; primer and intermediate are selected separately to suit the exposure.