640
640 is a Glass flake coating from Hempel. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 100% |
|---|---|
| Dry film thickness | 500 µm |
| Theoretical spreading rate | 2 m²/L |
| VOC | 24 g/L (China) |
| Density / specific gravity | 1.3 kg/L |
| Number of components | Two-component |
| Colour / appearance | Light Blue 36641 |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
Glass-flake coatings do not rely on thickness for their barrier; they rely on overlap. Countless glass flakes lie parallel in the film and stretch the permeation path many times over. In flue-gas desulphurisation, tank internals and chemical ponds they are close to standard practice. They also carry the highest application demands of the group.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Flake size and loadingFlake size trades barrier efficiency against workability. Large flakes barrier better but settle and are hard to pump; small flakes spray well but barrier less.
- Design thickness and coat countThese systems often run to several hundred microns and need dedicated airless equipment plus multiple coats.
- Chemical resistance list with concentration and temperatureFGD, acids, alkalis and solvents each map to specific grades. They are not interchangeable.
- Curing conditions and post-treatmentMost need elevated temperature to reach their chemical resistance; ambient-cure versions perform lower.
Application control points
Dedicated equipment is mandatory
Glass flake wears pumps and tips hard. Ordinary spray gear fails within hours and delivers uneven output, which scrambles flake orientation.
Cross-spray every coat
A single direction lines the flakes up in one plane and drops barrier performance. Crossing passes build the interleaved structure.
Spark testing is a required check
Lining work is tested for holidays to the relevant standard, and repairs are made before acceptance.
How to settle site disputes
Treating glass flake as ordinary epoxy
Windows, equipment and curing all differ. A crew set up for normal epoxy will generate a high rework rate.
Insufficient thickness allows permeation
The barrier is the number of overlapping layers. Too thin means too few layers and the medium travels along the channels between flakes.
Common questions on this coating class
Can glass-flake coatings be used for potable water?
What are the advantages over rubber or plastic lining?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.
Need the original TDS or a quote for this model?
Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.