MODEL DATA

Hardtop Optima Alu

BrandJotun
ModelHardtop Optima Alu
CategoryPolysiloxane topcoat

Hardtop Optima Alu is a Polysiloxane topcoat from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids74 ± 2%
Dry film thickness65–100 µm
Theoretical spreading rate11.4–7.4 m²/L
VOC159 g/L (US)
Density / specific gravity1.2 kg/L
Number of componentsTwo-component
ThinnerJotun Thinner No. 17
Mixing ratio4 parts: 1 part (by volume)

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Polysiloxane topcoats sell on high solids plus weathering: one coat can reach a substantial thickness, cutting coat count and schedule. Curing runs through siloxane hydrolysis and condensation and needs moisture from the air, so the humidity requirement is inverted compared with most coatings. Too dry and it does not cure.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Solid content and VOCHigh solids is the advantage over polyurethane, and it maps directly to emissions compliance and coat count. The figure must be measured, not theoretical.
  2. Humidity requirement for cureA minimum relative humidity is needed to finish curing. Dry regions and sealed spaces require humidification.
  3. Recoat windowUsually wider than polyurethane, but past the limit abrasion is still required.
  4. Required primer systemUsually epoxy or MIO epoxy intermediate. The wrong system shows up as intercoat adhesion failure.

Application control points

Raise humidity, do not add thinner

When cure looks slow, the common error is adding thinner to help it dry, which disrupts crosslinking. Increase ambient humidity or reschedule.

Control the pass on a high-build coat

High solids means short flow time. Distance, pass speed and overlap have to be right first time; rework marks are hard to remove.

Remove contamination inside the window

The cured surface is dense. Contamination that sits before the next coat becomes a weak boundary.

How to settle site disputes

Applying at low temperature and high humidity

It needs moisture, but that does not permit work near dew point. Substrate below dew point fails the same way as any other coating.

Treating high solids as permission to skip a coat

Fewer coats only works if the single-coat thickness is met and even. Where it runs thin, weathering life is set by the thinnest point.

Common questions on this coating class

How many coats of polysiloxane?
Most systems specify one, provided the thickness is achieved in that pass. Where thickness control is critical, two coats are safer.
How does it compare with fluorocarbon?
Both are top-tier weathering materials. Polysiloxane gives up some gloss retention to fluorocarbon but needs fewer coats at higher solids, which often wins on total cost.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Typically used as a topcoat for colour, gloss and weatherability; primer and intermediate are selected separately to suit the exposure.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← JOTUN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp