PPG PSX 500
PPG PSX 500 is a Polysiloxane topcoat from PPG. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 76 ± 2% |
|---|---|
| Dry film thickness | 50–75 µm (2.0–3.0 mil) per coat |
| Theoretical spreading rate | 15.2 m²/L |
| VOC | Max 142.0 g/kg |
| Density / specific gravity | 1.4 kg/L (11.3 lb/US gal) |
| Number of components | Two-component |
| Thinner | 0–5%, depending on the required film thickness and application conditions |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
Polysiloxane topcoats sell on high solids plus weathering: one coat can reach a substantial thickness, cutting coat count and schedule. Curing runs through siloxane hydrolysis and condensation and needs moisture from the air, so the humidity requirement is inverted compared with most coatings. Too dry and it does not cure.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Solid content and VOCHigh solids is the advantage over polyurethane, and it maps directly to emissions compliance and coat count. The figure must be measured, not theoretical.
- Humidity requirement for cureA minimum relative humidity is needed to finish curing. Dry regions and sealed spaces require humidification.
- Recoat windowUsually wider than polyurethane, but past the limit abrasion is still required.
- Required primer systemUsually epoxy or MIO epoxy intermediate. The wrong system shows up as intercoat adhesion failure.
Application control points
Raise humidity, do not add thinner
When cure looks slow, the common error is adding thinner to help it dry, which disrupts crosslinking. Increase ambient humidity or reschedule.
Control the pass on a high-build coat
High solids means short flow time. Distance, pass speed and overlap have to be right first time; rework marks are hard to remove.
Remove contamination inside the window
The cured surface is dense. Contamination that sits before the next coat becomes a weak boundary.
How to settle site disputes
Applying at low temperature and high humidity
It needs moisture, but that does not permit work near dew point. Substrate below dew point fails the same way as any other coating.
Treating high solids as permission to skip a coat
Fewer coats only works if the single-coat thickness is met and even. Where it runs thin, weathering life is set by the thinnest point.
Common questions on this coating class
How many coats of polysiloxane?
How does it compare with fluorocarbon?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Typically used as a topcoat for colour, gloss and weatherability; primer and intermediate are selected separately to suit the exposure.
Need the original TDS or a quote for this model?
Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.