MODEL DATA

Pilot ACR

BrandJotun
ModelPilot ACR
CategoryAcrylic coating

Pilot ACR is a Acrylic coating from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids55 ± 2%
Dry film thickness60–120 µm
Theoretical spreading rate9.2–4.6 m²/L
VOC400 g/L (China)
Density / specific gravity1.5 kg/L
Number of componentsOne-component
ThinnerJotun Thinner No. 7 /Jotun Thinner

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Acrylic coatings film by solvent evaporation: fast drying, easy recoating, decent colour retention, a common choice for maintenance and temporary protection. The weak points are solvent and chemical resistance, and long immersion. Whether it fits depends on exposure severity, not on price.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Thermoplastic or thermosetting (with hardener)Single-component thermoplastic acrylic films by solvent loss and resists solvents poorly; two-component acrylic (acrylic polyurethane) is a grade higher. Both get called acrylic.
  2. Weathering grade and recommended exposureC2–C3 atmosphere is its home ground; used alone above C4, life is short.
  3. Recoating intervalThermoplastic acrylic dries very fast; past the interval it needs solvent softening or abrasion, otherwise intercoat adhesion is poor.
  4. VOC and solidsSolvent-borne acrylic runs high on VOC; export projects need to check destination limits.

Application control points

Fast drying is an advantage and a trap

Drying too fast under-levels the film and leaves orange peel; on thick coats the surface seals and solvent cannot escape. Slow the pass down a notch.

Do not apply over alkyd or oil-based old paint

The solvent lifts the old film and wrinkles it. Where the existing system is unknown, test a small area first.

Blend repairs across a whole elevation

Colour retention is moderate and spot repairs show. Blend along a joint or over the full face.

How to settle site disputes

Single-component acrylic in heavy-duty service

It is not a long-life anti-corrosion coating, especially in industrial or coastal atmosphere. Those cases call for epoxy primer plus polyurethane topcoat.

Over-thinning causing poor film formation

Thinning to stretch the paint leaves low thickness and collapses weathering performance, with nothing visible on the surface. Stay within the TDS limit.

Common questions on this coating class

Can acrylic be used as temporary protection?
Yes: fast, recoatable, low cost, suitable between process stages. It is not a long-term system, so replace it with the specified topcoat before handover.
How does it differ from polyurethane?
One grade lower on solvent and chemical resistance and on gloss retention, and one grade lower in price. Fine indoors and in mild atmosphere; not for exposed heavy-duty work.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Typically used as a topcoat for colour, gloss and weatherability; primer and intermediate are selected separately to suit the exposure.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← JOTUN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us