Resist 65

BrandJotun
ModelResist 65
CategoryZinc-rich primer

Resist 65 is a Zinc-rich primer from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids72 ± 2%
Dry film thickness50–90 µm
Theoretical spreading rate14.4–8 m²/L
VOC366 g/L (China)
Density / specific gravity2.4 kg/L
Number of componentsTwo-component
ThinnerTo accelerate evaporation
Mixing ratio9 parts: 2 parts (by volume)

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Zinc-rich primers do not protect by sealing the steel; they protect because zinc corrodes before steel does. Zinc particles in the dry film touch each other and remain electrically connected to the substrate, so the corrosion current consumes zinc first and the steel stays cathodically protected. That path requires three things at once: zinc content, conductivity and adhesion. Lose any one and the coat becomes an ordinary pigmented paint.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Zinc content in the dry filmWhether the figure is by weight or by volume, and to which standard, must be stated. SSPC Paint 20 and ISO 12944-5 set different thresholds for the word zinc-rich, so a bare claim of high zinc means nothing.
  2. Type: epoxy or inorganic zinc silicateThe curing chemistry is entirely different. Epoxy cures by chemical crosslinking; inorganic zinc cures by silicate condensation and needs moisture to complete. Treating them alike leads directly to wrong site decisions.
  3. Minimum surface preparationMost require abrasive blast to Sa 2.5 with a medium profile. Below that grade the zinc never reaches clean steel and cathodic protection never starts.
  4. Recommended DFT range and maximum per coatToo thick and zinc-rich films crack, especially inorganic types; too thin and the zinc particles stop touching. Both limits belong in the data sheet.
  5. Overcoating interval and surface preparation before overcoatingInorganic zinc forms white zinc salts in damp conditions; these must be removed and the surface abraded before the next coat. Data sheets often compress this into a single word.
  6. Curing conditions (temperature and humidity window)Inorganic zinc silicate needs humidity to cure and cures poorly when too dry; epoxy types stall at low temperature.

Application control points

Hold the window between blasting and painting

Blasted steel starts to rust within hours in damp air. Painting zinc-rich over that rust puts zinc on oxide, the electrical path breaks and the coat is wasted. On fabrication work, keep blasting, coating and drying in one rhythm; it is far cheaper than reblasting later.

Mixing and filtration decide zinc distribution

Zinc is dense and settles fast. Circulation time, agitation and filter mesh follow the TDS; otherwise the top and bottom of a drum carry different zinc levels and one wall ends up with two different coatings. Thick coats make it worse.

Pinholes and dry spray are the classic defects

Fog, wind and long spray distance produce dry spray with through-pinholes. Zinc-rich films have little barrier effect, so corrosion starts at each pinhole and creeps inward. A holiday check after spraying costs far less than recoating a whole elevation.

The overcoating window matters most on inorganic zinc

Its cure is an irreversible silicate condensation. Leave it too long and a dense silicate skin forms; topcoat adhesion drops sharply. Past the window the only route is abrasion and re-coat, not a simple touch-up.

How to settle site disputes

Higher zinc is not better

Zinc content and service life are not linear. Excess zinc costs adhesion and crack resistance, particularly at high film build and low curing temperature. Select on exposure and system, not on the biggest number.

Blistering and cracking are often blamed on the wrong thing

Blisters in a zinc-rich layer usually mean moisture in the substrate or in the air got sealed in, not that the paint was off-spec; cracking is usually excessive single-coat thickness or incomplete cure at low temperature. Measure thickness and moisture before discussing material.

Common questions on this coating class

Epoxy zinc or inorganic zinc?
It depends on the downstream system and the temperature. Inorganic zinc takes higher heat and solvents better but needs humidity to cure and is sensitive to the overcoating window; epoxy zinc is more forgiving on site and holds adhesion steadily, which suits tight fabrication schedules. Marine atmospheric zones and tank exteriors often differ; decide on the system, not the single coat.
Can a zinc-rich primer be used as a finish?
No. The film is porous, with gaps between zinc particles. Exposed to UV and rain it chalks and loses zinc quickly. An intermediate and a topcoat belong in the system.
How do I read a zinc-content test report?
Check the method (weight or volume), whether the sample was dry film or wet paint, and the standard number. The same product can produce different figures under different methods; a report without the method cannot be compared.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Typically used as a primer for adhesion and corrosion protection; compatibility with intermediates and topcoats follows the manufacturer's system.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← JOTUN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp