MODEL DATA

SteelMaster 1200WF

BrandJotun
ModelSteelMaster 1200WF
CategoryFire protection

SteelMaster 1200WF is a Fire protection from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids69 ± 3%
Dry film thickness210–690 µm
VOC39 g/L (China)
Density / specific gravity1.4 kg/L
Number of componentsOne-component
ThinnerFresh water

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Fire protection coatings are fire safety products, not ordinary paints. Performance is fixed by type approval plus the certified system, and the relationship between thickness and fire rating is locked at testing time. It cannot be adjusted on site. That sets the selection logic: certification scope first, price second.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Approval type and scope of applicationThe substrate type, section factor and fire rating covered by the test report must match the actual project. Outside that scope the product is not valid.
  2. Thickness-to-rating tableThat table is part of the certification, not a recommendation. Work back from the required rating; do not estimate from experience.
  3. Intumescent or non-intumescentIntumescent is thin, looks better and suits internal steel; non-intumescent cementitious is thick and used outdoors, for hydrocarbon fires and in tunnels.
  4. Compatible primer and topcoatFire coatings place specific demands on the primer, whose expansion behaviour affects char formation.

Application control points

Follow the certified documents for preparation and primer

The primer type named in the report cannot be swapped; changing it steps outside the certification.

Measure every member and judge on the thinnest point

Beams, nodes, bolts and stiffeners vary widely. Acceptance is on the minimum, not the average.

Respect temperature and humidity limits

Intumescent coatings are sensitive to humidity and drying rate, and crack when applied thick. Build in coats with controlled intervals.

How to settle site disputes

Mixing thickness tables between manufacturers

Fire performance is a certified system result and cannot be transferred between similar products. Changing maker means new approval.

Using anti-corrosion paint as fire protection

The purposes differ. An anti-corrosion system provides no fire rating and will fail fire acceptance.

Common questions on this coating class

Can thickness be calculated in-house?
No. Thickness comes from the table in the type test report, read against member type, section factor and rating. It is not estimated from area or experience.
Does steel fire protection need a topcoat?
Not in dry indoor conditions. Outdoors, in damp or corrosive conditions a compatible topcoat is required, and it must appear in the certified system.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← JOTUN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp