Key technical data

Volume solids49 ± 2%
Dry film thickness40-70 µm/coat
Theoretical spreading rate7.0 m²/L /70 µm
VOC500 g/L
Number of componentsOne-component
ThinnerChlorinated rubber thinner
Mixing ratioOne-component

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Chlorinated rubber is single-component and solvent-evaporative: fast drying, usable at low temperature, good water and alkali resistance, once the mainstay of marine and chemical environments. Two practical issues remain: high VOC, and chlorinated formulations restricted by environmental rules in some markets. Confirm the destination allows it before selecting.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. VOC and local regulatory limitsChlorinated coatings face restrictions or declaration duties in some countries; export projects must check first.
  2. Compatibility with primer and topcoatIt works over itself, epoxy and bitumen, but not over alkyd or oil-based films, which it lifts.
  3. Minimum application temperatureLow-temperature application is one of its advantages, but the floor differs by product.
  4. Weathering and colour retentionLong exposure dulls and shifts colour; accept that in a topcoat or switch to polyurethane.

Application control points

Solvent release means separate coats

A single heavy coat traps solvent and leaves pinholes and retained solvent. Several thin coats is standard.

Low temperature is not high humidity tolerance

In damp air the surface condenses and the film hazes. The dew point criterion still applies.

Identify the old coating before repair

Chlorinated rubber cannot go directly over alkyd. A small test patch is the cheapest way to find out.

How to settle site disputes

Ignoring the regulatory risk

Shipping into a market that restricts chlorinated coatings can stall at customs or at acceptance. That is compliance, not quality.

Treating fast drying as fewer steps

Fast drying shortens waiting, not the required coat count or thickness.

Common questions on this coating class

Is chlorinated rubber still usable?
In markets that permit it, yes, especially for low-temperature work and fast-turnaround maintenance. Check destination rules first.
How does it compare with acrylic?
Better water and alkali resistance, slightly higher cost, more environmental pressure. Inland and coastal maintenance still commonly use chlorinated rubber or modified systems.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← KANSAI Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp