EPP301
EPP301 is a Shop primer from Osaka. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 25% |
|---|---|
| Dry film thickness | 25 µm corresponds to 100 µm WFT |
| Theoretical spreading rate | 8.7 m²/kg |
| VOC | 645 g/L |
| Density / specific gravity | Approx. 1.15 kg/L |
| Number of components | Two-component |
| Thinner | OUP 106, recommended addition 3%–5% |
| Mixing ratio | Component A: Component B = 15:6.4 (by weight) |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
A primer has two jobs: hold onto the steel and keep water and oxygen out. It carries no weathering duty and no appearance duty, so it is judged on adhesion, flash-rust resistance and compatibility with what comes next, not on gloss or colour.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Required surface preparation grade and profilePrimers split into tolerant (rust-tolerant, moisture-tolerant) and blast-only types. That difference decides whether a blasting machine goes to site, and it moves the application cost in the quote.
- Flash-rust resistance and recoat windowThe key figures for shop primers and temporary protection. If the steel will rust between blasting and topcoating, choose a flash-rust resistant grade or the intermediate step is wasted.
- Compatibility with the topcoat systemData sheets list recommended systems. Cross-brand combinations need separate confirmation; alkyd over epoxy or chlorinated rubber under polyurethane are the classic adhesion failures.
- Recommended DFT and maximum per coatToo thick and intercoat adhesion suffers; too thin and the barrier is incomplete. Edges, welds and bolts typically reach only about sixty percent of the flat-area thickness.
Application control points
Stripe coat edges and welds first
Spray shadows leave edges, bolts and welds below design thickness, and that is exactly where corrosion starts. Codes call for a stripe coat. Skipping it returns later as rework at several times the cost.
Thin only with the specified thinner at the specified ratio
A cheaper solvent looks fine for weeks, then intercoat adhesion drops and the film lifts. The paint gets blamed; the thinner did it.
Watch dew point and substrate temperature
Substrate temperature must sit safely above dew point or the surface condenses and water sits under the film. ISO 12944 and the data sheets state the criterion; measure it with a meter, not by hand.
How to settle site disputes
Rust-tolerant does not mean no preparation
These products tolerate thin, tight rust, not heavy scale, flaking or oil. Treating tolerance as an exemption from preparation is the most common misuse.
Intercoat adhesion failures rarely show up on the day
Primer-to-topcoat breakdown usually appears two or three months later as large clean peels. Look at whether the peeled face is paint-on-paint or paint-on-steel; that tells you whether the system or the preparation is at fault.
Common questions on this coating class
Can a single primer coat be handed over?
How do I reduce cross-brand system risk?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Typically used as a primer for adhesion and corrosion protection; compatibility with intermediates and topcoats follows the manufacturer's system.
Need the original TDS or a quote for this model?
Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.