Key technical data

Volume solids48% ± 2%
Dry film thickness35 µm (1.4 mils) per coat
Theoretical spreading rate13.7 m²/L
VOCMaximum value 345.0 g/kg
Density / specific gravity1.2 kg/L (10.0 lb/US gal)
Number of componentsOne-component
ThinnerThinner 20-05

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Alkyds cure by oxidation: unsaturated fatty acids in the resin crosslink with atmospheric oxygen. Cheap, easy to apply, single-component and glossy, they are the highest-volume traditional anti-corrosion coating. Two hard limits are alkali and long immersion: applied directly to new concrete, galvanised steel or alkaline substrates they saponify and lift.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Long, medium or short oil lengthOil length sets drying speed, flexibility and weathering. Long oil is flexible and weathers well but dries slowly; short oil is hard, fast and weathers poorly. The applications differ completely.
  2. Whether galvanised steel or new concrete is permittedMost alkyds do not resist alkali and saponify on direct application. A dedicated primer or a different system is required.
  3. Recommended DFT and coat countSingle alkyd coats should not be thick: skin dry over soft material wrinkles. Several thin coats is the correct method.
  4. Thinner typeUse the specified alkyd thinner. The wrong solvent drops the resin out of solution or causes very slow drying.

Application control points

Thin coats with real intervals

Oxidative drying is gradual. Coating over touch-dry seals solvent into the first coat and produces wrinkling and poor adhesion over time.

Cold and damp slows drying badly

The oxidation reaction crawls at low temperature and high humidity, so dust and rain land on a wet film. Reschedule or change system.

Identify the existing coating before recoating

Alkyd over epoxy or polyurethane adheres poorly; epoxy over alkyd lifts the old film. Both directions need checking.

How to settle site disputes

Alkyd in immersion or buried service

In long immersion alkyd blisters and detaches. That is a system selection error, not an application error.

Price as the only criterion

Alkyd has the lowest unit price, but refurbishment cycles in heavy-duty areas are short, so whole-life cost is usually higher.

Common questions on this coating class

Is alkyd still usable on steel structures?
In mild atmosphere (C1–C2), indoors and in non-immersion areas, yes, with a complete primer system. Heavy-duty work has moved to epoxy and polyurethane.
Why does alkyd fall off new galvanising?
The zinc surface is alkaline and saponifies the fatty acids, leaving a loose layer. A dedicated galvanised-steel primer or an epoxy system is needed.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← PPG Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp