MODEL DATA

5908A SEA GRANDPRIX MARK II

BrandCMP
Model5908A SEA GRANDPRIX MARK II
CategoryAntifouling

5908A SEA GRANDPRIX MARK II is a Antifouling from CMP. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids55 ± 2% (by volume) (ISO 3233)
Dry film thickness75–160 µm
Theoretical spreading rate0.136-0.291 L/m²
VOC425 g/L (Method24)
Density / specific gravity1.76g/ml (ISO:2811)
Number of componentsOne-component
ThinnerCR/ACRI THINNER A
Colour / appearanceBrown, light brown

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Antifouling is not anti-corrosion. It deals with marine growth, while corrosion protection comes from the system below it. Effectiveness depends on the controlled release of biocide from the film, and release rate is set by thickness and resin type. Film thickness is therefore a design parameter, not a box to tick.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Mechanism (self-polishing, contact, foul-release)The three suit different speeds, idle periods and routes. Self-polishing suits high speed and long voyages, foul-release suits frequent berthing, contact types suit slow short trips.
  2. Design thickness against service yearsAntifouling life is essentially thickness times biocide loading. Thin or missed areas fail first and collect growth.
  3. Required sealer or tie coatAntifouling cannot go straight onto epoxy without a tie layer; adhesion and biocide migration both suffer. The manufacturer specifies the system.
  4. Maximum exposure before launchOverexposed antifouling loses effect. Past the limit it must be recoated, not launched.

Application control points

Record thickness by area, not as an average

Flat bottom, bilge, topsides and running gear see different flow and carry different requirements. A single average figure is no record at all.

Overlap wet-on-wet

Where an overlap dries before the next pass, the seam becomes the weak point and the first place growth appears.

Lock the launch window

There is an upper limit between the last coat and launch. Yard schedules squeeze that window, so fix it early.

How to settle site disputes

Blaming paint quality for poor antifouling

Most early failures come from low thickness, poor overlaps or late launch. The failure pattern, patchy or uniform, points back to the cause.

Mixing antifouling brands

Different biocide systems combine into an uncontrolled release rate that either underperforms or depletes early. One system per hull.

Common questions on this coating class

Can antifouling go over old antifouling?
Depends on type and condition. The same type in good condition can be overcoated after low-pressure washing; a different type must be removed completely or the intercoat fails.
Is antifouling for inland vessels the same as for ocean-going ships?
No. Inland craft run slow with long idle periods, where foul-release or low-release types fit better; long ocean voyages usually use self-polishing. Select on the operating profile, not the price.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Typically used below the waterline for antifouling; the system and application window depend on trading area, speed and dock schedule.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← CMP Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us