MODEL DATA

8052 CERABEST Grey

BrandCMP
Model8052 CERABEST Grey
CategoryHeat-resistant coating

8052 CERABEST Grey is a Heat-resistant coating from CMP. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids42 ± 2%
Dry film thickness30 µm
Theoretical spreading rate0.071 L/m²
VOC554 g/L
Density / specific gravity1.51 g/mL
Number of componentsTwo-component
ThinnerINORGANIC SHOP THINNER Series
Mixing ratioSlurry: base = 44:56 (by volume)
Colour / appearanceGrey

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Heat-resistant coatings are mostly silicone-based: the high bond energy of Si–O resists thermal ageing, and some products add aluminium pigment for higher temperature plus a dense oxide layer. The key is not one temperature figure but how temperature, duration and thermal cycling combine.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Continuous versus short-term peak temperatureThe two must be read separately and they differ widely. Selecting on peak temperature is a common error.
  2. Aluminium pigment, and which typeAluminium grades take more heat but need care in welding and cutting; non-aluminium colours accept less heat and offer more colour choice.
  3. Required preparation and primerMost systems need a high blast grade, and the primer must also be heat resistant. An ordinary primer fails first at temperature.
  4. Heating curve (whether staged bake-out is required)Ramping too fast on first heat causes blistering and cracking. Data sheets usually give a staged schedule.

Application control points

Follow the staged ramp on first heat

Freshly applied heat-resistant paint releases residues on first heating. Too fast and volatiles blow through as bubbles and pinholes.

Keep the film thin

Thick silicone films crack under thermal cycling. Several thin coats beat one thick one.

Poor preparation delaminates first at temperature

Thermal expansion and contraction amplify weak adhesion. Blast grade and profile both have to be met.

How to settle site disputes

Selecting on peak temperature

An occasional excursion is not the normal condition. Select on continuous temperature and check the peak separately.

Using an ordinary anti-corrosion primer underneath

At temperature the epoxy carbonises first and the topcoat comes off in sheets. The whole system must be heat resistant.

Common questions on this coating class

Can heat-resistant paint go directly on bare steel?
Some products can, but most need a heat-resistant primer for adhesion and corrosion protection. Follow the manufacturer's system.
Does colour affect heat resistance?
Dark colours absorb more heat, so the surface runs hotter than a light colour. Light or aluminium colours suit hot equipment, subject to the colour range in the TDS.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← CMP Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp