Heat-resistant coatings: the temperature rating is only the entry ticket
Nobody selects a heat-resistant coating on temperature alone. Continuous temperature, peak temperature, thermal cycling and the attacking medium — four conditions decide whether a grade works. 87 models.
Separate continuous from peak temperature first. A silicone coating rated 400 °C means continuous service; a short excursion to 500 °C may be fine, but repeated peaks accelerate resin degradation. Reading the peak figure as continuous is the most common misuse of this product family.
Second, thermal cycling. Expansion and contraction from start-stop cycles turn the difference in elongation between coating and steel into interfacial shear. Flues, exhaust ducts and cracking furnaces that cycle often fail sooner than a furnace held at constant temperature — the same coating may last eight years on constant duty and three on frequent cycling before it lifts.
Third, the medium. High temperature plus sulphur, plus chlorine, plus hydrogen are entirely different corrosion mechanisms. Silicone aluminium coatings resist high-temperature oxidation but are attacked in sulphur-bearing flue gas, where a ceramic-filled or flue-gas-specific system is needed. Same temperature, different medium, opposite answer.
Application is where this family fails most. Most silicone products do not cure, or cure extremely slowly, at ambient temperature — the first heat-up does the curing. If the equipment's first ramp is too steep, solvent and moisture cannot escape and the film blisters over large areas. Follow the maker's staged ramp curve with holds at the critical temperatures.
All models in this group
Grouped by brand. Open a model for technical data, system position and in-category alternatives.
OSAKA 24
JOTUN 15
PPG 14
T&H 9
CMP 6
KANSAI 5
Tell us your substrate and service conditions
One-to-one coating consultancy: system design, quantity take-off and quotation.