Pilot QD Topcoat
Pilot QD Topcoat is a Alkyd coating from Jotun. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 44 ± 2% |
|---|---|
| Dry film thickness | 30–60 µm |
| Theoretical spreading rate | 14.3-7.4 m²/L |
| VOC | 514 g/L |
| Density / specific gravity | 1.3 kg/L |
| Number of components | One-component |
| Thinner | JOTUN Thinner No. 7 |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
Alkyds cure by oxidation: unsaturated fatty acids in the resin crosslink with atmospheric oxygen. Cheap, easy to apply, single-component and glossy, they are the highest-volume traditional anti-corrosion coating. Two hard limits are alkali and long immersion: applied directly to new concrete, galvanised steel or alkaline substrates they saponify and lift.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Long, medium or short oil lengthOil length sets drying speed, flexibility and weathering. Long oil is flexible and weathers well but dries slowly; short oil is hard, fast and weathers poorly. The applications differ completely.
- Whether galvanised steel or new concrete is permittedMost alkyds do not resist alkali and saponify on direct application. A dedicated primer or a different system is required.
- Recommended DFT and coat countSingle alkyd coats should not be thick: skin dry over soft material wrinkles. Several thin coats is the correct method.
- Thinner typeUse the specified alkyd thinner. The wrong solvent drops the resin out of solution or causes very slow drying.
Application control points
Thin coats with real intervals
Oxidative drying is gradual. Coating over touch-dry seals solvent into the first coat and produces wrinkling and poor adhesion over time.
Cold and damp slows drying badly
The oxidation reaction crawls at low temperature and high humidity, so dust and rain land on a wet film. Reschedule or change system.
Identify the existing coating before recoating
Alkyd over epoxy or polyurethane adheres poorly; epoxy over alkyd lifts the old film. Both directions need checking.
How to settle site disputes
Alkyd in immersion or buried service
In long immersion alkyd blisters and detaches. That is a system selection error, not an application error.
Price as the only criterion
Alkyd has the lowest unit price, but refurbishment cycles in heavy-duty areas are short, so whole-life cost is usually higher.
Common questions on this coating class
Is alkyd still usable on steel structures?
Why does alkyd fall off new galvanising?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.
Need the original TDS or a quote for this model?
Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.