PPG SIGMALINE 780 PHENGUARD SUBSEA 780
PPG SIGMALINE 780 PHENGUARD SUBSEA 780 is a Phenolic epoxy from PPG. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.
Key technical data
| Volume solids | 66 ± 2% |
|---|---|
| Dry film thickness | 100–175 µm (4.0–7.0 mils) depending on coating system requirements |
| Theoretical spreading rate | 6.6 m²/L |
| VOC | 300.0 g/L (2.5 lb/gal) |
| Density / specific gravity | 1.7 kg/L (14.2 lb/US gal) |
| Number of components | Two-component |
| Thinner | Thinner 91-92 |
| Colour / appearance | Shades RAL 1004, RAL 1018, RAL 2004 |
The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.
How this coating class protects
Phenolic epoxy is not a better epoxy; it is a different route. Higher functionality raises crosslink density substantially, which lifts the starting point for solvent, acid and heat resistance. The price is brittleness and a stricter curing temperature. It appears in chemical tanks, tank linings, pipe internals and solvent-resistant floors, not on ordinary exterior walls.
What to verify in the original TDS
These are checking criteria, not numeric commitments. Every figure follows the current original TDS.
- Minimum curing temperature and post-cure requirementThis is where phenolic epoxy most often fails. At low temperature the crosslinking is incomplete, chemical resistance drops a grade and nothing shows on the surface.
- Chemical resistance list with concentration and temperature limitsResistance is always conditional: a given acid at a given concentration below a given temperature. A bare claim of acid and alkali resistance has no engineering meaning.
- Recommended DFT and number of coatsLining work often runs to several hundred microns and needs multiple coats or high-build airless spray. Forcing that thickness in one coat cracks.
- Whether a topcoat or seal coat is requiredPhenolic epoxy chalks under UV. Exposed or open-air areas need a separate topcoat.
Application control points
Curing temperature is the first gate
A shop that can heat the substrate and a site that cannot are two different selections. If site temperature cannot reach the minimum, change the system or change the schedule; extending drying time does not fix it.
Thickness and holiday testing are mandatory
Lining failures are usually through-pinholes, not large-scale detachment. Spark testing after spray is standard practice on this work.
Surface preparation has to be at the top grade
Phenolic epoxy serves aggressive media; Sa 2.5 is the floor and many projects specify Sa 3. Without the profile, adhesion will not survive long immersion.
How to settle site disputes
Substituting ambient-cure for heat-cure
It looks identical and performs very differently. The medium permeates, blisters form, then detachment; repair means relining the whole tank.
Ignoring the real operating temperature of the medium
Design temperature is given at the maximum, and operation often exceeds it. Margin at selection beats extra thickness afterwards.
Common questions on this coating class
Can phenolic epoxy be used for potable water or food contact?
Why does the same paint last in a tank but chalk outdoors in two years?
The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.
Place in the coating system
Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.
Need the original TDS or a quote for this model?
Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.