MODEL DATA

ZD6340

BrandZINDN
ModelZD6340
CategoryBitumen coating

ZD6340 is a Bitumen coating from ZINDN. This page groups model identity, system position and the data request entry so you can verify the full system before enquiring.

Key technical data

Volume solids80% ± 2%
Dry film thickness100µm
Theoretical spreading rate215 g/m²
Density / specific gravity1.5 ± 0.1
Number of componentsTwo-component
ThinnerX-500 Epoxy Thinner
Mixing ratioOne-component
Colour / appearanceBlack

The technical content below is reproduced in English as published by the manufacturer; terms, grades and values follow the English original.

How this coating class protects

Bituminous coatings win on water resistance, resistance to dilute acids and alkalis, and cost. They are common on buried pipe, piling, sewage tanks and damp substrates. The limits are equally clear: poor solvent resistance, poor UV resistance, strong temperature sensitivity. Three questions decide fit: sunlight, solvents, temperature.

What to verify in the original TDS

These are checking criteria, not numeric commitments. Every figure follows the current original TDS.

  1. Epoxy-modified or straight bitumenEpoxy bitumen is clearly stronger mechanically and chemically, at higher cost. The two are not comparable.
  2. Temperature range (softening point and low-temperature embrittlement)Bitumen is temperature sensitive: it flows when hot and cracks when cold. Buried and exposed service differ.
  3. Whether a topcoat is requiredExposed to UV it ages, so a topcoat or a modified grade is needed.
  4. Tolerance of damp substratesSome products apply on damp surfaces, which is their advantage over epoxy, but damp is not the same as wet.

Application control points

Judge substrate moisture against the TDS

Damp tolerance has limits. Free water and seepage must be dealt with.

Build real thickness

The barrier comes from thickness. A thin bitumen coat achieves nothing.

Protect before backfill

Buried sections are easily damaged by stone during backfill; add a protection layer or bedding.

How to settle site disputes

Exposed use without a topcoat

UV ageing cracks the surface, water enters the cracks and protection ends.

Contact with solvents or oils

Bitumen dissolves or softens. Those environments need epoxy or glass flake.

Common questions on this coating class

Epoxy bitumen or straight bitumen?
Choose epoxy bitumen where mechanical strength and chemical resistance matter; straight bitumen is enough for plain waterproofing where cost dominates.
Can bitumen be used in potable water tanks?
Generally not advised. Judge on the specific product's approval and consider odour and leaching.

The above gives class-level technical requirements and judging methods. Specific values and systems follow the current original TDS and the project specification.

Place in the coating system

Primer–intermediate–topcoat layers and coat counts follow the exposure; DFT and curing conditions follow the original TDS and project specification.

Need the original TDS or a quote for this model?

Send the model, quantity, destination port and service conditions — we reply with a complete coating system, not a single can.

← ZINDN Back to product catalog →
Need selection advice?

Tell us your substrate and service conditions

One-to-one coating consultancy: system design, quantity take-off and quotation.

Contact us
WhatsApp